Daren Wu
Kelsey B. Hatzell
2025_DarenWu_KelseyHatzell_EES.Batteries_d5eb00097a ← click to see all uploads from this cell
2026-08-14 15:06:34
7c4e854a-d019-47ca-96ff-9d5a37867ed9
How to Cite
1 — Cite the dataset paper
↗ View paper
2 — Cite the ESRA platform
Galib, M. et al. (2026). ESRA: Energy Storage Research Assistant. Argonne National Laboratory. https://github.com/MusannaGalib/esra-platform
CC BY 4.0  ·  Data shared under Creative Commons Attribution 4.0

Location on Eagle / Perlmutter

/global/cfs/cdirs/m4845/gsharing/kelsey-b-hatzell/chemo-mechanical-limitations-of-liquid-a/2025-darenwu-kelseyhatzell-eesbatteries/DW1_85D3_NaK80 SGEIS & plating GEIS/cycling/ESRA-CYC-0012/
Open in Globus File Manager →

Linked Uploads

Type Group Date Project Link
XCT Kelsey B. Hatzell 2026-08-14 15:06 Chemo-mechanical limitations of liquid alloy anodes for sodium solid-state batteries same cell
EIS Kelsey B. Hatzell 2026-08-14 15:06 Chemo-mechanical limitations of liquid alloy anodes for sodium solid-state batteries same cell
EIS Kelsey B. Hatzell 2026-08-14 15:06 Chemo-mechanical limitations of liquid alloy anodes for sodium solid-state batteries same cell
Cycling Kelsey B. Hatzell 2026-08-14 15:06 Chemo-mechanical limitations of liquid alloy anodes for sodium solid-state batteries same cell
Cycling Kelsey B. Hatzell 2026-08-14 15:06 Chemo-mechanical limitations of liquid alloy anodes for sodium solid-state batteries same cell
Cycling Kelsey B. Hatzell 2026-08-14 15:06 Chemo-mechanical limitations of liquid alloy anodes for sodium solid-state batteries same cell
Cycling Kelsey B. Hatzell 2026-08-14 15:06 Chemo-mechanical limitations of liquid alloy anodes for sodium solid-state batteries same cell

Experiment Metadata

Visibility public
Electrolyte Na₃Zr₂Si₂PO₁₂ (NASICON) with 20 nm SnO₂ coating
Anode Material Na-K liquid alloy
Publication Doi 10.1039/d5eb00097a
Number Of Cycles run until short-circuit; pulsed stripping: multiple pulses (varies per rest condition)
Cathode Material Na metal
Institution Code ESRA
Electrode Area Cm2 0.503
Voltage Window — Upper 3.0
Current / C-Rate / Protocol Summary CCD: 0.05, 0.1, 0.2, 0.4 mA cm⁻² (Na stripping/plating); SGEIS: 0.05–1 mA cm⁻², step 0.01 mA cm⁻²; pulsed: 1 mA cm⁻², 1 s pulse + 0.1–10 s rest