Katherine Steinberg
Betar Gallant
2025_KatherineSteinberg_BetarGallant_ACS.Energy.Lett._5c01274 ← click to see all uploads from this cell
2026-08-12 21:51:56
c4848812-829f-49bc-8c24-57070547af74
How to Cite
1 — Cite the dataset paper
↗ View paper
2 — Cite the ESRA platform
Galib, M. et al. (2026). ESRA: Energy Storage Research Assistant. Argonne National Laboratory. https://github.com/MusannaGalib/esra-platform
CC BY 4.0  ·  Data shared under Creative Commons Attribution 4.0

Location on Eagle / Perlmutter

/global/cfs/cdirs/m4845/gsharing/betar-gallant/deciphering-unresolved-materials-in-quan/2025-katherinesteinberg-betargallant-acs/01_BATTERY_CYCLING/cycling/ESRA-CYC-0001/
Open in Globus File Manager →

Linked Uploads

Type Group Date Project Link
SEM Betar Gallant 2026-08-14 12:55 Deciphering Unresolved Materials in Quantitative Analysis of Lithium Metal Solid Electrolyte Interphases same cell
NMR Betar Gallant 2026-08-12 21:52 Deciphering Unresolved Materials in Quantitative Analysis of Lithium Metal Solid Electrolyte Interphases same cell
ICP Betar Gallant 2026-08-12 21:52 Deciphering Unresolved Materials in Quantitative Analysis of Lithium Metal Solid Electrolyte Interphases same cell
GC Betar Gallant 2026-08-12 21:51 Deciphering Unresolved Materials in Quantitative Analysis of Lithium Metal Solid Electrolyte Interphases same cell

Experiment Metadata

Visibility public
Electrolyte Multiple: LP40; LiFSI DME; LiDFOB + LiBF₄ FEC/DEC; LiFSI DME/TTE LHCE
Temperature C 25.0
Anode Material Li chips (99.9%, 16 mm × 0.6 mm, MTI Corp; rolled to ~4× original size)
Publication Doi 10.1021/acsenergylett.5c01274
Number Of Cycles Variable per electrolyte to achieve 0.6–0.8 mAh total capacity loss (LP40: 4; LiFSI DME: 6; LiDFOB+LiBF₄: 9; LiFSI LHCE: 12 for ¹H-NMR)
Cathode Material Cu foil (16 mm diameter, working electrode)
Institution Code ESRA
Electrode Area Cm2 0.0
Voltage Window — Lower 0.0
Voltage Window — Upper 1.0
Theoretical Capacity Mah 3860.0
Current / C-Rate / Protocol Summary Constant-capacity galvanostatic protocol; 5 h initial rest; j = 0.5 mA/cm², Q = 1 mAh/cm²; stripped to 1 V vs. Li; 5 min rest between each half cycle